Compression Strength : ≥40-80 kPa
Water Absorption : ≤0.4 kg/m2
Payment Terms : L/C,T/T
Point Load : ≥200-700 N
Density : 120-180 kg/m³
Hydrophobic Rate : ≥99.0%
Place of Origin : china
Thermal Conductivity : ≤0.040 W/m*K
MOQ : 1 container.
Our high compressive strength roof fireproof rock wool is engineered for airport terminals, convention centers, and large transportation hubs with large-scale roofing systems. Featuring high-density rock wool formed through 3D pleating technology with excellent compressive strength, ensuring long-term stability under combined equipment loads, maintenance loads, and wind loads.
| Parameter Product | HR120 | HR140 | HR160 | HR180 |
|---|---|---|---|---|
| Density (kg/m³) | 120 | 140 | 160 | 180 |
| Compression Strength (kPa) | ≥40 | ≥45 | ≥60 | ≥80 |
| Point Load (N, Deformation: 5 mm) | ≥200 | ≥260 | ≥500 | ≥700 |
| Thermal Conductivity (W/m*K, 25°C) | ≤0.040 | |||
| Combustibility | Class A1 non-combustible | |||
| Acidity Coefficient | ≥2.0 | |||
| Hydrophobic Rate (%) | ≥99.0 | |||
| Water absorption (kg/m², short term, partial immersion) | ≤0.4 | |||
| Mass moisture absorption (%) | ≤0.3 | |||

|
|